ICS 21.060.01
CCS J 13
中华人民共和国国家标准
GB/T 5267.5—2024
紧固件表面处理
第5 部分:热扩散渗锌层
Fasteners surface treatment—Part 5:Zinc thermal diffusion coatings
2024-09-29 发布2025-04-01 实施
国家市场监督管理总局
国家标准化管理委员会发 布
目 次
前言 ····································································································· Ⅲ
引言 ····································································································· Ⅳ
1 范围 ·································································································· 1
2 规范性引用文件 ······················································································ 1
3 术语和定义 ··························································································· 1
4 渗锌层体系和工艺 ···················································································· 2
5 耐腐蚀性和渗锌层等级 ··············································································· 3
6 尺寸要求和测量 ······················································································ 4
7 机械、物理性能和试验 ··············································································· 5
8 紧固件渗锌层体系标记 ··············································································· 6
9 订货信息 ······························································································ 6
10 储存条件 ···························································································· 6
附录A (资料性) 热扩散渗锌层等级推荐应用 ······················································· 7
参考文献 ·································································································· 8
前 言
本文件按照GB/T 1.1—2020《标准化工作导则 第1 部分:标准化文件的结构和起草规则》的规
定起草。
本文件是GB/T 5267《紧固件表面处理》的第5 部分。GB/T 5267 已经发布了以下部分:
—GB/T 5267.1 紧固件 电镀层;
—GB/T 5267.2 紧固件 非电解锌片涂层;
—GB/T 5267.3 紧固件 热浸镀锌层;
—GB/T 5267.4 紧固件表面处理 耐腐蚀不锈钢钝化处理;
—GB/T 5267.5 紧固件表面处理 第5部分:热扩散渗锌层。
请注意本文件的某些内容可能涉及专利。本文件的发布机构不承担识别专利的责任。
本文件由中国机械工业联合会提出。
本文件由全国紧固件标准化技术委员会(SAC/TC 85)归口。
本文件起草单位:中机生产力促进中心有限公司、上海高强度螺栓厂有限公司、定西高强度紧固件
股份有限公司、舟山市7412 工厂、绍兴山耐高压紧固件有限公司、山东高强紧固件有限公司、中国电
力科学研究院有限公司、明阳智慧能源集团股份公司、河北信德电力配件有限公司、苏州热工研究院有
限公司、盐城科奥机械有限公司、中广核风电有限公司、浙江烨凌实业有限公司、舟山市正山智能制造
科技股份有限公司、雁栖湖基础制造技术研究院(北京)有限公司、中车青岛四方机车车辆股份有限公
司、江苏中成紧固技术发展股份有限公司、重庆标准件工业有限责任公司、国智科技(河北)股份有限
公司、邯郸市兆运电力紧固件制造有限公司、山东鲁电线路器材有限公司、宁波世裕五金电器有限公
司、杭州华佳标准件有限公司、安徽宏源铁塔有限公司、上海达克罗涂复工业有限公司、宁波市镇海甬
鼎紧固件制造有限公司、株洲春华实业有限责任公司、浙江新盛达金属科技发展股份有限公司、中国第
一汽车股份有限公司、中国汽车技术研究中心有限公司、上海集优张力控制螺栓有限公司、奇瑞汽车股
份有限公司。
本文件由全国紧固件标准化技术委员会负责解释。
引 言
紧固件表面处理是紧固件生产中重要的环节,根据涂覆层功能可实现紧固件耐腐蚀性、装饰性和功
能性要求。螺纹紧固件在选择表面处理时,不仅要实现各种功能作用,同时还要满足螺纹旋合性要求。
GB/T 5267 旨在规范针对紧固件产品的电镀层、非电解锌片涂层、热浸镀锌层、不锈钢钝化和热扩散渗
锌层等不同表面处理的技术要求,为涂料供应商、涂镀层加工方、紧固件制造者、分销商和最终用户组
织生产、销售和产品质量验收检查提供标准依据,拟由5 个部分构成:
—GB/T 5267.1 紧固件 电镀层(ISO 4042);
—GB/T 5267.2 紧固件 非
CCS J 13
中华人民共和国国家标准
GB/T 5267.5—2024
紧固件表面处理
第5 部分:热扩散渗锌层
Fasteners surface treatment—Part 5:Zinc thermal diffusion coatings
2024-09-29 发布2025-04-01 实施
国家市场监督管理总局
国家标准化管理委员会发 布
目 次
前言 ····································································································· Ⅲ
引言 ····································································································· Ⅳ
1 范围 ·································································································· 1
2 规范性引用文件 ······················································································ 1
3 术语和定义 ··························································································· 1
4 渗锌层体系和工艺 ···················································································· 2
5 耐腐蚀性和渗锌层等级 ··············································································· 3
6 尺寸要求和测量 ······················································································ 4
7 机械、物理性能和试验 ··············································································· 5
8 紧固件渗锌层体系标记 ··············································································· 6
9 订货信息 ······························································································ 6
10 储存条件 ···························································································· 6
附录A (资料性) 热扩散渗锌层等级推荐应用 ······················································· 7
参考文献 ·································································································· 8
前 言
本文件按照GB/T 1.1—2020《标准化工作导则 第1 部分:标准化文件的结构和起草规则》的规
定起草。
本文件是GB/T 5267《紧固件表面处理》的第5 部分。GB/T 5267 已经发布了以下部分:
—GB/T 5267.1 紧固件 电镀层;
—GB/T 5267.2 紧固件 非电解锌片涂层;
—GB/T 5267.3 紧固件 热浸镀锌层;
—GB/T 5267.4 紧固件表面处理 耐腐蚀不锈钢钝化处理;
—GB/T 5267.5 紧固件表面处理 第5部分:热扩散渗锌层。
请注意本文件的某些内容可能涉及专利。本文件的发布机构不承担识别专利的责任。
本文件由中国机械工业联合会提出。
本文件由全国紧固件标准化技术委员会(SAC/TC 85)归口。
本文件起草单位:中机生产力促进中心有限公司、上海高强度螺栓厂有限公司、定西高强度紧固件
股份有限公司、舟山市7412 工厂、绍兴山耐高压紧固件有限公司、山东高强紧固件有限公司、中国电
力科学研究院有限公司、明阳智慧能源集团股份公司、河北信德电力配件有限公司、苏州热工研究院有
限公司、盐城科奥机械有限公司、中广核风电有限公司、浙江烨凌实业有限公司、舟山市正山智能制造
科技股份有限公司、雁栖湖基础制造技术研究院(北京)有限公司、中车青岛四方机车车辆股份有限公
司、江苏中成紧固技术发展股份有限公司、重庆标准件工业有限责任公司、国智科技(河北)股份有限
公司、邯郸市兆运电力紧固件制造有限公司、山东鲁电线路器材有限公司、宁波世裕五金电器有限公
司、杭州华佳标准件有限公司、安徽宏源铁塔有限公司、上海达克罗涂复工业有限公司、宁波市镇海甬
鼎紧固件制造有限公司、株洲春华实业有限责任公司、浙江新盛达金属科技发展股份有限公司、中国第
一汽车股份有限公司、中国汽车技术研究中心有限公司、上海集优张力控制螺栓有限公司、奇瑞汽车股
份有限公司。
本文件由全国紧固件标准化技术委员会负责解释。
引 言
紧固件表面处理是紧固件生产中重要的环节,根据涂覆层功能可实现紧固件耐腐蚀性、装饰性和功
能性要求。螺纹紧固件在选择表面处理时,不仅要实现各种功能作用,同时还要满足螺纹旋合性要求。
GB/T 5267 旨在规范针对紧固件产品的电镀层、非电解锌片涂层、热浸镀锌层、不锈钢钝化和热扩散渗
锌层等不同表面处理的技术要求,为涂料供应商、涂镀层加工方、紧固件制造者、分销商和最终用户组
织生产、销售和产品质量验收检查提供标准依据,拟由5 个部分构成:
—GB/T 5267.1 紧固件 电镀层(ISO 4042);
—GB/T 5267.2 紧固件 非
相关推荐
- GB/T 15135-2018 燃气轮机 词汇
- GB/T 13002-2022 旋转电机 热保护
- GB∕T 12818-2021 铁路客车组装后的检查与试验规则
- GB∕T 40424-2021 管与管板的焊接工艺评定试验
- GB/T 41160-2022 铸造工具钢
- GB/T 25334.2-2023 铁路机车车体 第2部分:电力机车
- GB/T 29716.1-2013 机械振动与冲击 信号处理 第1部分:引论
- GB/T 10322.7-2016 铁矿石和直接还原铁 粒度分布的筛分测定
- GB∕T 18998.2-2022 工业用氯化聚氯乙烯(PVC-C)管道系统 第2部分:管材
- GB/Z 3480.22-2024 直齿轮和斜齿轮承载能力计算 第22部分:微点蚀承载能力计算